发明名称 SEMI-CRYSTALLINE, SEMI-AROMATIC TERPOLYMERS WITH SUPERIOR POST-MOLDING SHRINKAGE AND MECHANICAL PERFORMANCE
摘要 <p>This invention relates to high temperature, semi-crystalline, semi-aromatic nylon terpolymers with improved shrinkage resistance, made from terephthalic acid (TA), hexamethylene diamine (HMD) and/or 2-methyl pentamethylene diamine (2-MPMD) and another aliphatic dicarboxylic acid as monomers. These polymers display superior % TD (Transverse Direction) annealing shrinkage, as well as very good balance of mechanical performance as high temperature nylons.</p>
申请公布号 WO1997043330(A1) 申请公布日期 1997.11.20
申请号 CA1997000334 申请日期 1997.05.16