摘要 |
The invention provides a polymerizable composition formed by mixing a liquid and a powder composition. The liquid composition includes a peroxide, which decomposes by at most fifty percent by weight of the peroxide within 10 hours at a temperature of at least 75 DEG C., and a polymerizable monomer. The powder composition comprising a proton donor, and a metal containing compound. The polymerizable composition has from 0.2 to 5 percent by weight of the peroxide, from 5 to 99 percent by weight of the polymerizable monomer, and from 0.1 to 3 percent by weight of the proton donor, and from 0.02 to 3 percent by weight of the metal containing compound. The polymerizable composition has an initial setting time and a storage setting time after storage of the first (liquid) composition for at least 12 months at a temperature of at least 23 DEG C. The initial setting time is within 2 minutes of the storage setting time.
|