A method for producing an enhanced adsorbent and/or enhanced catalytic particle and/or for producing a catalytic particle, comprising the steps of: (a) removing an effective amount of air from a closed chamber containing an adsorbent and/or catalytic particle, wherein the resultant chamber pressure is less than one atmosphere; (b) raising the chamber pressure with an inert gas to at least one atmosphere; (c) contacting the particle with an energy beam of sufficient energy for a sufficient time to thereby enhance the adsorbent and/or catalytic properties of the particle and/or produce catalytic properties in the particle. A continuous process directed to step (c) alone is also provided. Also disclosed are adsorbent and/or catalytic particles, methods of contaminant reduction or elimination, including room temperature catalysis, particle binders, apparatuses of the present invention, and methods of increasing the surface area of adsorbent and/or catalytic particles. |
申请公布号 |
ZA9603056(B) |
申请公布日期 |
1997.11.05 |
申请号 |
ZA19960003056 |
申请日期 |
1996.04.17 |
申请人 |
M & K PATENT COMPANY, INC. |
发明人 |
MARK L. MOSKOVITZ;BRYAN E. KEPNER |
分类号 |
A61L9/00;B01D53/02;B01D53/86;B01D53/94;B01J3/00;B01J3/02;B01J19/08;B01J19/24;B01J20/30;B01J20/34;B01J21/04;B01J23/34;B01J37/34;C01B31/08;C02F1/28 |
主分类号 |
A61L9/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|