摘要 |
PROBLEM TO BE SOLVED: To obtain a transparent laminated body with excellent environmental durability by using a non-crystalline oxide thin film mainly consisting of indium and tin and with a specified resistance for an intermediate transparent high refractive index layer and the uppermost transparent high refractive index layer. SOLUTION: A laminated body is prepd. by forming successively at least a transparent high refractive index layer 20, a metal thin film layer 30 and a transparent high refractive index layer 40 on one of the main face of a transparent base body 10. In this case, a non-crystalline oxide thin film formed under high oxygen concn. atmosphere by a sputtering method and mainly consisting of indium and tin and with a specific resistance of at least 1×10<-2>Ω.cm is used for the transparent high refractive index layers 20 and 40. A metal with a small electric specific resistance is pref. used for the metal thin film layer 30 placed between the transparent high refractive index layers 20 and 40.
|