A pressurized water reactor ("PWR") radial reflector fabricated of 20% to 30% cold worked AISI Type 316 stainless steel blocks will experience about 0.14% volumetric swelling at a neutron dose level of about 100 dpa at retirement. The reflector will not be susceptible to swelling-embrittlement at retirement.
|