发明名称 Sätt att utveckla resttryckspänning i rostfritt stål och nickelbaserade varmhållfasta legeringar samt reparation av utav spänningskorrosion framkallade sprickor genom svetsning under vattnet
摘要 The method concerns development of compressive residual stresses in corrosion resistant steels and superalloys on nickel basis. It consists of producing a bath of molten metal, cooling the bath to build a metallurgical bond with adjoining solid metal, and quenching the bonded metal to the temperature of the surroundings below the melting zone of the metal through contact with a quenching medium. Also claimed are a method for repair of damage caused stress corrosion cracks, and a corresponding apparatus.
申请公布号 SE9701239(L) 申请公布日期 1997.10.09
申请号 SE19970001239 申请日期 1997.04.04
申请人 GEN ELECTRIC 发明人 SOLOMON HARVEY DONALD;WHITE RAYMOND ALAN;FUSARO JR ROBERT ANTHONY
分类号 G21D1/00;B23K9/00;B23K9/23;B23K10/02;B23K31/00;C21D1/00;C21D1/09;C21D6/00;C21D9/50;C22F1/00;C22F1/10;(IPC1-7):C21D9/50 主分类号 G21D1/00
代理机构 代理人
主权项
地址