摘要 PROBLEM TO BE SOLVED: To improve the tenacity of this molded article by using a thermoplastic polymer composition, which is obtained by adding the specific ratio of the specified addition polymerization block copolymer during the manufacturing reaction of polyester resin. SOLUTION: An addition polymerization block copolymer is at least one kind of block copolymer selected from the group comprising a block copolymer B1 and a block copolymer B2. The block copolymer B1 is the block copolymer having at least one kind of polymer block selected from the group consisting of a polymer block mainly made of aromatic vinyl compound unit and a polybutadiene block having below 30% of hydrogenated 1,2-linkage amount, a polybutadiene block having 30-80% of hydrogenated 1,2-linkage amount and a hydrogenated isoprene/butadiene copolymer block. The block copolymer B2 is a block copolymer having a polymer block mainly made of aromatic vinyl compound unit and a polyisobutyl block.
申请公布号 JPH09262896(A) 申请公布日期 1997.10.07
申请号 JP19960099082 申请日期 1996.03.28
申请人 KURARAY CO LTD 发明人 OMOTO MINORU;ISHIDA MASAO;ISHINO SHUHEI;KAWAHARA SHIGERU
分类号 C08J5/00;B29C49/00;B29K67/00;B29L22/00;C08L53/00;C08L67/00;(IPC1-7):B29C49/00 主分类号 C08J5/00
代理机构 代理人
主权项
地址