摘要 |
In the deinking of feed waste papers comprising magazines and newspapers at a weight ratio of magazine to newspaper of from 5/95 to 60/40, a reclaimed pulp with excellent qualities can be obtained by adjusting the treating temperature in the flotation step to 40 DEG to 80 DEG C. and adding a deinking agent, which contains an alkylene oxide adduct of an oil or fat, wherein said alkylene oxide adduct comprises ethylene oxide and propylene oxide added at a molar ratio of ethylene oxide to propylene oxide of from 1/1 to 5/1, and has a cloud point of 45 DEG to 90 DEG C., at least in one of the steps of the deinking process.
|