摘要 |
<p>PROBLEM TO BE SOLVED: To obtain a microwave-weldable resin compsn. which exhibits a high heat exchange rate and provides a high amt. of heat and of which the heat generation can be easily controlled, enabling the prevention of degradation of the resin, by compounding a thermoplastic resin with fine conductive aniline polymer particles and a conductive inorg. powder. SOLUTION: This compsn. comprises 100 pts.wt. thermoplastic resin, 5-100 pts.wt. fine conductive aniline polymer particles, and 3-50 pts.wt. conductive inorg. powder, the content of the polymer particles being higher than that of the inorg. powder. Examples of the resin are a polyolefin resin (e.g. polyethylene or polypropylene), a vinyl chloride resin, and an acrylic resin. Examples of the inorg. powder are barium titanate, titanium oxide, a metal powder such as of copper or zinc, and carbon black.</p> |