发明名称
摘要 <p>The invention relates to a deflection ring of sintered MgZn-ferrite material. In accordance with the invention, this deflection ring is characterized in that the majority of the grains of the sintered material have a monodomain structure. By virtue thereof, a relatively small heat dissipation occurs in the ring when it is used in a cathode ray tube. The average grain size of the sintered MgZn-ferrite material is preferably 2.8 micrometers or less. MgZn-ferrite materials whose composition corresponds to the formula Mg1-zZnzFe2-yO4, wherein 0.1<z<0.4 and 0.01<y<0.3, have the additional advantage that they have a relatively high saturation magnetization and a relatively high electrical resistance. The invention also relates to a cathode ray tube comprising the above-mentioned deflection ring and to a mo1lding made from the above-mentioned MgZn-ferrite material.</p>
申请公布号 JPH09507960(A) 申请公布日期 1997.08.12
申请号 JP19960515873 申请日期 1995.10.25
申请人 发明人
分类号 C04B35/26;H01F1/34;H01F41/02;H01J29/76;(IPC1-7):H01J29/76 主分类号 C04B35/26
代理机构 代理人
主权项
地址