摘要 |
A method for making a synthetic meixnerite which, when activated, has a high B.E.T. surface area, typically about 290 m2/g or greater. The method comprises activating hydrotalcite, then cooling and hydrating such activated material in a carbon dioxide-free environment. Such hydration can produce a material that absorbs more than 100% of its weight in water. Following hydration, this material is activated a second time in a virtually carbon dioxide-free environment.
|