发明名称 |
Low-friction ceramics |
摘要 |
The present invention provides a low-friction ceramic having a lowered coefficient of friction and an enhanced strength. The ceramic comprises as the matrix phase a nonoxide ceramic containing silicon, such as Si3N4 or SiC and an iron compound in an amount of about 5 to 40% by weight dispersed in the matrix phase. This ceramic is excellent in the ability to adsorb lubricating oil, has a low coefficient of friction, is almost free from pores, and has a strength equal to or higher than that of a ceramic containing no iron oxide.
|
申请公布号 |
US5643842(A) |
申请公布日期 |
1997.07.01 |
申请号 |
US19950510873 |
申请日期 |
1995.08.03 |
申请人 |
ISUZU CERAMICS RESEARCH INSTITUTE CO., LTD. |
发明人 |
UNNO, YASUAKI;YAMAMURO, HIDEO;KITA, HIDEKI |
分类号 |
C04B35/565;C04B35/575;C04B35/584;C04B35/593;C04B35/597;C04B35/78;F16C33/04;(IPC1-7):C04B35/565;C04B35/599 |
主分类号 |
C04B35/565 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|