发明名称 PROCESS FOR PREPARING ANTISTATIC POLYESTER FIBER
摘要 The vessel where polyethylene terephthalate oligomer is stored is kept to 260 degree C, while the slurry, in which terephthalic acid and ethylene glycol are compounded is fed into the vessel for 6 hours to obtain an oligomer, then is delivered to another polymer vessel. Correspondingly, the compound of formula(1) and (2) are reacted at 80-100 degree C in the vessel, therein the additive and the catalyst are added in small amount, and is processed with the polymerization at 280 degree C to obtain a polyester polymer, and spun, drawn in such method that the polyester fiber is produced.
申请公布号 KR970010712(B1) 申请公布日期 1997.06.30
申请号 KR19940028643 申请日期 1994.11.02
申请人 TONGYANG POLYESTER CO.,LTD 发明人 SIM, CHOONG-BO;KIM, MOON-CHAN
分类号 D01F1/10;D01F6/62;(IPC1-7):D01F1/10 主分类号 D01F1/10
代理机构 代理人
主权项
地址