摘要 |
The invention relates to a microcellular PU elastomer with improved dynamic-mechanical characteristics, based on an isocyanate component consisting essentially of 4,4'-MDI and other standard components. The elastomer in question has a physical-chemical structure characterised by a one- or two-peak signal next to the low-molecular main signal for an (apparent) molar mass of greater than 250,000 g/mol as measured by gel-permeation chromatography from a solution of the microcellular PU elastomer produced at 90 DEG C in N,N-dimethylformamide with 1 % di-n-butylamine, against polymethylmethacrylate (PMMA) as the standard, the signal being reduced or eliminated following addition of lithium chloride to this solution. The elastomer has a urea content of 14-18 wt %. Also disclosed are a process for producing such a microcellular PU elastomer with improved dynamic-mechanical characteristics and the use of said elastomer to produce damping elements.
|
申请人 |
BASF AG, 67063 LUDWIGSHAFEN, DE |
发明人 |
KRECH, RUEDIGER, 49356 DIEPHOLZ, DE;ROTERMUND, UDO, DR., 01990 ORTRAND, DE;BOLLMANN, HEINZ, 49594 ALFHAUSEN, DE;HEMPEL, RENATE, 01987 SCHWARZHEIDE, DE;SCHOLZ, WOLFGANG, 49448 LEMFOERDE, DE;GENZ, MANFRED, DR., 49401 DAMME, DE |