PROBLEM TO BE SOLVED: To give transparency, functionality and designedness to this plate-like body by a method wherein a reinforced resin composition, in which the specified weight percentage of this plate-like molding of a glass filler having a refractive index smaller or larger than that of an aromatic polycarbonate resin by a specified value or less and a specified weight percentage of this plate-like molding of polycaprolactone are blended with each other. SOLUTION: Between two transparent thermoplastic resin films or sheets, a reinforced resin composition, which is prepared by blending an aromatic polycarbonate resin, 1-60wt.% (of a plate-like molding) glass filler having a refractive index smaller or larger than that of the aromatic polycarbonate resin by 0.015 or less and 1-60wt.% (of the plate-like molding) polycaprolatone to one another, is melted, injected and filled. Thus, the composition is laminated to the film or sheet into an integral body. Concretely, between two transparent thermoplastic resin films or sheets 1 and 1', a reinforced resin composition layer 2 integrally laminated to the films or sheets is formed. |