When using this procedure in the production of plan-convex lens, the precisely measured quantity of the monomer mixture, containing the polymerisation catalyst,is coated on the horizontal smooth template, the surface of which is drenched closed to the angle greater than 0, and after that it is undertaken to the polymerisation conditions in the inert atmosphere.
|