摘要 A method of treating titanium-containing parts and the parts so-treated, which treatment includes placing the parts in a furnace chamber (12) having a gaseous atmosphere of 15-25 % carbon monoxide, 30-50 % nitrogen and 30-50 % hydrogen, are disclosed, The atmosphere is at a temperature of between 1450-1850 DEG F and the treatment lasts for 5-300 minutes. Parts experience improved hardness, strength and wear resistance.