发明名称 |
One part room temperature vulcanizing composition having both a high rate of extrusion and low sag |
摘要 |
A method for producing a room temperature vulcanizable composition that has a high rate of extrusion and a low sag wherein a base mixture of a diorganopolysiloxane and an end stopping cross linking ketoximosilane are reacted prior to being added to a first injection port along an extruder, an inorganic filler being added to said base mixture at a second injection port along the extruder, an M stopped silicone fluid being partitioned into two parts and the first part of said M stopped fluid being added to the filler containing base mixture at a third injection port at the middle of the extruder, and a tin catalyst, an adhesion promoter and the second part of the M stopped fluid being added at a fourth injection port along the extruder said mixture comprising these components being extruded towards the extruder exit port.
|
申请公布号 |
US5616647(A) |
申请公布日期 |
1997.04.01 |
申请号 |
US19960589521 |
申请日期 |
1996.01.22 |
申请人 |
GENERAL ELECTRIC COMPANY |
发明人 |
DZIARK, JOHN J.;PINK, MICHAEL R.;MARTUCCI, JOHN P. |
分类号 |
C08L83/04;(IPC1-7):C08K3/26;C08L83/06 |
主分类号 |
C08L83/04 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|