发明名称 |
POLYPROPYLENE RESIN COMPOSITION |
摘要 |
PROBLEM TO BE SOLVED: To obtain the subject composition excellent in impact resistance, rigidity and heat resistance. SOLUTION: This resin composition 0.5-300g/10min in MFR determined in accordance with the JIS K-7210 comprises (A) 70-95wt.% of a homopolypropylene component 0.01-1000g/10min in MFR satisfying the relationship:ΔHm >=24.50+1.583logMFR (ΔHm is heat of fusion determined by differential scanning colorimetry) and (B) 5-30wt.% of a propylene-ethylene copolymer component 30-80wt.% in ethylene content and 2-6dl/g in intrinsic viscosity.
|
申请公布号 |
JPH0987445(A) |
申请公布日期 |
1997.03.31 |
申请号 |
JP19950266521 |
申请日期 |
1995.09.20 |
申请人 |
TONEN CHEM CORP |
发明人 |
MORIYA MASAYUKI;SAKURAI KENICHI;OKADA KOJI;NAKAJIMA MASASHI |
分类号 |
C08L23/10;C08L23/00;(IPC1-7):C08L23/10 |
主分类号 |
C08L23/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|