摘要 |
PCT No. PCT/FR94/00311 Sec. 371 Date Jan. 30, 1995 Sec. 102(e) Date Jan. 30, 1995 PCT Filed Mar. 22, 1994 PCT Pub. No. WO94/22779 PCT Pub. Date Oct. 13, 1994The invention relates to a method for fabricating laminated glazing comprising at least one enamel layer, wherein is deposited an enamelled composition comprising an anti-adhesive frit, a medium and, optionally, a low melt point frit on a portion of the internal face of a glass sheet; the enamelled glass sheet is subjected to heat treatment at a temperature between 150 DEG C. and the glass deformation temperature, and a second glass sheet is placed on the enamelled side of the first glass sheet before simultaneous bending of the two glass sheets, final firing of the enamel taking place during bending.
|