发明名称 |
Method of reducing the bubble formation when curing a room temperature vulcanizable silicone sealant composition with silicon-bonded alkoxy crosslinker on a hot porous surface |
摘要 |
Bubble formation observed when curing a sealant composition on a hot porous substrate is reduced where the room temperature vulcanizable silicone sealant composition comprises a polydiorganosiloxane, a crosslinker with silicon-bonded alkoxy groups, filler, and a titanium catalyst by the addition of 0.5 to 2 weight percent of an oximosilicon compound.
|
申请公布号 |
US5565541(A) |
申请公布日期 |
1996.10.15 |
申请号 |
US19950464180 |
申请日期 |
1995.06.05 |
申请人 |
DOW CORNING CORPORATION |
发明人 |
CARBARY, LAWRENCE D.;KLOSOWSKI, JEROME M. |
分类号 |
C09K3/10;C08K5/54;C08L83/02;C08L83/04;(IPC1-7):C08G77/08 |
主分类号 |
C09K3/10 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|