摘要 |
<p>A magnetic recording medium includes a flexible substrate (10), a coating layer (20) formed on the flexible substrate (10), and a magnetic layer(30) formed on the coating layer(20). The coating layer(20) contains a binder and nonmagnetic particles and has a thickness in the range of 0.05 to 0.7 mu m as a result of a stretching treatment performed at least once after application of the coating layer on the flexible substrate. The magnetic layer(30) contains magnetic powder, a binder and an abrasive and has a thickness in the range of 0.05 to 1.0 mu m. The nonmagnetic particles contained in the coating layer has an average particle size in the range of 0.01 to 0.08 mu m. The abrasive contained in the magnetic layer has an average particle size in the range of 0.05 to 0.8 mu m and satisfies conditions defined by the following equations (1) and (2): <MATH> <MATH> <MATH> wherein dmx represents a maximum particle size of the abrasive, dav represents an average particle size of the abrasive, tc represents a thickness of the coating layer, and tm represents a thickness of the magnetic layer. With this arrangement, the magnetic recording medium is excellent in productivity and further improves a surface property of the thin magnetic layer. This achieves high outputs at a region of shorter wavelength and further achieves excellent running durability.</p> |