发明名称 METHOD OF ALLOY COMPRISING AT LEAST TWO ALLOY COMPONENTS HAVING DIFFERENT MELTING POINTS
摘要 <p>In a process for the production of alloys from at least two alloy components (A, B, C, D, . . . ) with different melting points by melting in an inductively heated cold-walled crucible (1) with a cooled crucible base (3), in order to obtain an exact and homogeneous alloy composition at least a part of the alloy components (A, B, C, D, . . . ) are introduced into the cold-walled crucible (1) consecutively and in stacked fashion where either a) the alloy component (a) in each case with the lower melting point is introduced first or b) the alloy component in each case with the lower density is introduced first and following the introduction at least one of further alloy component the heating energy is switched on. The process serves preferably for the production of the intermetallic phase TiAl, where firstly the aluminium and then the titanium are stacked in the cold-walled crucible (1).</p>
申请公布号 JPH08246080(A) 申请公布日期 1996.09.24
申请号 JP19960021188 申请日期 1996.02.07
申请人 A L D BUAKIYUUMU TECHNOL GMBH 发明人 AROOKU CHIYAUDOURII;MATEIASU BURUUMU;HAARARUTO SHIYORUTSU;GEORUKU YARUCHIYUKU
分类号 C22C1/00;C21C5/52;C22C1/02;(IPC1-7):C22C1/02 主分类号 C22C1/00
代理机构 代理人
主权项
地址