摘要 |
Novel wear- and temper-resistant, high hot strength alloy has the compsn. (by wt.) 10-35% Mo and/or 20-50% W; 0.6-6% C; 5-25% V, Ti, Zr, Nb and/or Ta; 0-20% Cr; 0-12% Co; 0-8% Ni; 0-5% Si; 0-5% Al; 0-5% Mn; 0-5% Cu; 0-2% B; 0-0.5% N; balance at least 30% Fe and impurities, with the provisos that (a) the total Mo+W concn. has a minimum value increasing linearly from 10% to 20% with increasing W content and a max. value increasing linearly from 35% to 50% with increasing W content; (b) the ratio of C atoms to total number of V, Ti, Zr, Nb and/or Ta atoms is 0.5-2; and (c) the total Cr, Co, Ni, Si, Al, Mn, Cu, B and N concn. is max. 25%. Also claimed are prodn. processes for the above alloy in which the alloy is produced by melting or powder metallurgy and then either rapidly cooled or nitrided to increase wear resistance and strength.
|
申请人 |
PATENTSTELLE FUER DIE DEUTSCHE FORSCHUNG DER FRAUNHOFER-GESELLSCHAFT, 80636 MUENCHEN, DE |
发明人 |
LI, FENG, DIPL.-ING., 52070 AACHEN, DE |