发明名称 ALUMINUM ALLOY WITH IMPROVED TRIBOLOGICAL CHARACTERISTICS
摘要 An antifrictional aluminum alloy and a method for making an aluminum alloy without lead are provided. The alloy has improved tribological characteristics and a base composition, in weight percent as follows: silicon: 3.0-6.0; copper: 2.0-5.0; zinc: 0.5-5.0; magnesium: 0.25-0.5; nickel: 0.2-0.6; tin: 0.5-5.0; bismuth: 0.1-1.0; iron: up to 0.7; aluminum: essentially the balance.
申请公布号 WO9625527(A1) 申请公布日期 1996.08.22
申请号 WO1995US01843 申请日期 1995.02.14
申请人 CATERPILLAR INC.;BOURKHINA, ANNA N. 发明人 BOURKHINA, ANNA N.
分类号 C22C1/02;C22C21/00;C22C21/02;C22C21/14;(IPC1-7):C22C1/02;C22C1/03;C22B9/04;C22B9/05;C22B21/00;C22B21/06 主分类号 C22C1/02