发明名称 POLYOLEFIN COMPOSITION FOR INJECTION MOLDING
摘要 Compsn. comprises a super-high molecular weight polyolefin (1) (having a critical viscosity measured in decalin soln. at 135 deg. C of 10-40 dl/g (better 15-35 dl/g)) and a low and high molecular weight polyolefin (2) (having a critical viscosity measured in decalin at 135 deg. C of less than 10 dl/g (better 0.1-5 dl/g, best 0.5-3 dl/g)). Polyolefin (1) makes up 15-40 wt.% (better 20-35 wt.%) of the total amount of polyolefins (1) and (2). The critical viscosity (etc.) of the compsn. measured in decalin soln. at 135 deg. C lies between 4.0-10 dl/g (better 4-9 dl/g), the melting torque (T1) of the compsn. is 4.5 Kg cm or less. Polyethylene is used as a typical polyolefin. The compsn. is produced in a multi-stage polymerisation process consisting of (i) a process to produce (1) and (ii) a process to produce (2). Process (i) is carried out in the presence of Ziegler catalyst comprising: (A) a highly active component contg. Mg, Ti and a halogen, (B) organic aluminium compounds. Process (ii) is carried out in the presence of hydrogen molecules.
申请公布号 EP0274536(B2) 申请公布日期 1996.07.03
申请号 EP19870904320 申请日期 1987.07.03
申请人 MITSUI PETROCHEMICAL INDUSTRIES, LTD. 发明人 HONMA, SHIRO;TOMINARI, KENICHI;KURISU, MASAYOSHI
分类号 C08L23/02;C08F2/00;C08F2/38;C08F4/00;C08F4/60;C08F4/64;C08F4/654;C08F8/00;C08F10/00;C08F10/02;C08F110/02;C08L23/00;C08L23/06 主分类号 C08L23/02
代理机构 代理人
主权项
地址