An oxide magnetic material provided by the present invention contains, as main components, 61 to 67 mol% of Fe2O3; 3 to 36 mol% of MnO; and 30 mol% or less of ZnO, and further contains, as sub-components, 0.05 to 0.5 wt% of CaO; and 0.005 to 0.2 wt% of SiO2. Such materials can further contain one or more kinds of oxides selected from the group consisting of ZrO2, HfO2, Ta2O5, Cr2O3, MoO3, WO3, Al2O3, Ga2O3, In2O3, GeO2, SnO2, Sb2O3 and Bi2O3. Such magnetic materials of the present invention have the advantages of having an extremely low magnetic loss even when used in the high frequency band and having a minimum magnetic loss at a temperature sufficiently higher than room temperature. Moreover, a switching power supply having a switching frequency of 300 kHz to 5 MHz is provided by using such magnetic materials as a magnetic core. <IMAGE>
|