摘要 |
This resin is composed of (a) 50-90 wt% styrene polymer made by mixing 60-85 wt% aromatic vinyl compound, cyanic vinyl monomer and 0-40 wt% another vinyl monomer, (b) 5-35 wt% CPE containing 20-40 wt% chlorine and (c) 5-35 wt% regenerated ethylene-prophylene rubber made by melting, and mixing ethylene-prophylene rubber, organic peroxide and reactive monomer with carboxyl group or anhydrous carboxyl group at the rate of 100 (wt): 0-2 (wt): 1-5 (wt) and (c) 0-10 wt% vinyl graft polymer. Meta-acryl acid ester monomer, maleimide and acrylimid can be used as another vinyl monomer among components of (a).
|