发明名称 |
DEOXIDATION METHOD OF LOW CARBON INGOT SLAG |
摘要 |
agitating molten steel slag in a bubbling stand; degassing in a vacuum state; putting Ti-providing source of below 100kg/ton slag in the molten steel slag when producing an ultimite low carbon molten steel contaning C of below 0.01 wt.%, Si of below 0.02 wt.%, Ti of 0.035-0.055 wt.%, and the balance Fe with inevitable impurities; deoxidizing molten steel slag by blowing inactive gases through bubbling lance for 1-3 minutes; and degassing in a vacuum state.
|
申请公布号 |
KR950012414(B1) |
申请公布日期 |
1995.10.17 |
申请号 |
KR19930029160 |
申请日期 |
1993.12.22 |
申请人 |
POSCO |
发明人 |
KANG, BONG - SU;PARK, BYONG - KON;LEE, BAEK |
分类号 |
C21C7/06;(IPC1-7):C21C7/06 |
主分类号 |
C21C7/06 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|