The soft Chinese ink is prepared by mixing 60 wt% carbon, 30 wt% PVA or glue as an adhesive, 3 wt% a perfume, 0.5 wt% magnesium carbonate, 0.5 wt% an antiseptics and 6 wt% water in a vessel, (b) pulverizing the mixture with a compressive roller for about 1 hr., (c) putting this soft Chinese ink paste in a tube or a vessel. |