摘要 The invention relates to ferrous metallurgy, specifically, to the composition of a charge for use in the production of steel, in particular steel smelting in electrical furnaces. The essence of the invention is the fact that the composite charge for smelting steel comprises an iron-carbon alloy and oxide material in the following proportions (in wt %): iron-carbon alloy 50-95, oxide material 5-50. The oxide material contains between 0.25 and 99.5 % free oxides of metals with an affinity with oxygen not greater than that of carbon. Use of the proposed composite charge in steel smelting reduces the smelting time and improves the quality of the grades of steel smelted, as well as broadening the range of grades of smelted metal.
申请公布号 RU2044061(C1) 申请公布日期 1995.09.20
申请号 RU19930040973 申请日期 1993.08.19
申请人 NAUCHNO-PROIZVODSTVENNOE MALOE PREDPRIYATIE "INTERMET-SERVIS" 发明人 DOROFEEV GENRIKH A;AFONIN SERAFIM Z;UTKIN YURIJ V;MAKUROV ALEKSANDR V;SITNOV ANATOLIJ G
分类号 C21C5/04;C21B13/00;C21C5/52 主分类号 C21C5/04
代理机构 代理人
主权项
地址