发明名称 Kautschukmischung.
摘要 <p>It has been determined that certain rubbery polymers having multiple glass transition temperatures can be utilized in making tires which have improved rolling resistance, improved wet skid resistance, and outstanding tread wear. These rubbery polymers are derived from at least one conjugated diolefin monomer, have a first glass transition temperature which is between -110 DEG C and -20 DEG C and have a second glass transition temperature which is between -50 DEG C and 0 DEG C. These rubber polymers can be homopolymers of conjugated diolefin monomers, copolymers of more than one conjugated diolefin monomer, or copolymers derived from at least one conjugated diolefin monomer and at least one vinyl aromatic monomer.</p>
申请公布号 DE3751163(T2) 申请公布日期 1995.08.31
申请号 DE19873751163T 申请日期 1987.09.15
申请人 THE GOODYEAR TIRE & RUBBER CO., AKRON, OHIO, US 发明人 HALASA, ADEL FARHAN, BATH OHIO 44210, US;GROSS, BILL BUD, STOW OHIO 44224, US;COX, JOEL LYNN, N. CANTON OHIO 44721, US;BALOGH, GEORGE FRANK, N.CANTON OHIO 44720, US
分类号 B60C1/00;C08F36/00;C08F236/04;C08F297/02;C08L9/00;C08L21/00;C08L53/00;(IPC1-7):C08L9/00 主分类号 B60C1/00
代理机构 代理人
主权项
地址