摘要 |
The Al-Si sintered alloy having good mechanical strength and elongation and is especially excellent in wear resistance, and a method for producing the same. The sintered alloy consists of 2.4-23.5% Si, 2-5% Cu, 0.2-1.5% Mg, 0.01-1% of transition metals and the balance of aluminum and unavoidable impurities, and has a dapple grain structure of an Al-solid solution phase and an Al-Si alloy phase containing dispersed pro-eutectic Si crystals having a maximum diameter of 5-60 mu m either in the whole body or in the surface contact portion, and the area ratio of the Al-solid solution phase in the grain structure is in the range of 20-80%. |
申请人 |
HITACHI POWDERED METALS CO., LTD.;HONDA GIKEN KOGYO KABUSHIKI KAISHA |
发明人 |
ISHIJIMA, ZENZO;ICHIKAWA, JUN-ICHI;SASAKI, SHUJI;SHIKATA, HIDEO;URATA, HIDEO, C/O HONDA R & D CO., LTD.;KAWASE, SHOJI, C/O HONDA R & D CO., LTD.;UEDA, JUN-ICHI, C/O HONDA R & D CO., LTD. |