发明名称 Method for TIG welding 1.25 Cr-0.5Mo steel pipe for which preheating and postheating treatments can be effectively omitted
摘要 This invention is of a Cr-Mo steel pipe of a wall thickness of 13 mm or less, containing C: 0.03-0.10 wt %, Si: 0.50-1.00 wt %, Mn: 0.30-0.60 wt %, P</=0.007 wt %, S</=0.020 wt %, Cr: 1.00-1.50 wt %, Mo: 0.45-0.65 wt %, Al: 0.002-0.010 wt % and N: 0.002-0.010 wt % and the remainder consisting of Fe and unavoidable impurities for which preheating and postheating treatments for the prevention of weld cracking and stress corrosion cracking can be effectively omitted, said steel pipe of this invention being suitable for steam piping applications such as STPA23 used in power generation plants, etc.