<p>In synthetic, substantially spherical crystal aggregates of xonotlite having a particle size of more than 20 microns, and preferably up to 150 microns, up to 30% of the silicon atoms can be replaced by titanium or zirconium atoms, and inert particles can be incorporated in the crystal aggregates.</p> |