发明名称 Fremgangsmåte for opparbeidelse av jarosittholdige rester
摘要 <p>To work up jarosite-containing residues to give usable products, the jarosite-containing residues and zinc sulphide-containing concentrates are stirred in dilute sulphuric acid having a content of 40 to 100 g/l of free sulphuric acid in an autoclave at an oxygen partial pressure of at least 1000 kPa and a temperature of 130 to 170 DEG C, the iron and zinc content of the residue and of the zinc sulphide-containing concentrate are substantially brought into solution, separation into solution and solid is effected after the pressure has been let down, the solution is passed into the bleaching circulation of a zinc electrolysis with precipitation of the iron in the form of haematite, the elemental sulphur is separated off from the solid and the residue is transported for further use.</p>
申请公布号 NO176524(C) 申请公布日期 1995.04.19
申请号 NO19900004301 申请日期 1990.10.03
申请人 RUHR-ZINK GMBH 发明人 ROPENACH, ADOLF VON;BOHMER, WINFRIED;GRIMM, HEINER
分类号 B03B9/04;B09B3/00;C01B17/02;C01B17/06;C22B;C22B3/00;C22B3/08;C22B7/00;C22B9/02;C22B19/20;C22B19/30;C25C1/00;C25C1/16;(IPC1-7):C22B3/08 主分类号 B03B9/04
代理机构 代理人
主权项
地址