发明名称 |
Förfarande för framställning av ett efter blandning i vatten snabbt härdbart hydrauliskt bindemedel |
摘要 |
<p>Method of making a rapidly hardening hydraulic binder for mixing with water, the hardened mass produced therefrom having a defined water resistance. Calcium sulphate alpha -hemihydrate is used as the rapidly hardening component in a predetermined starting quantity, the hardened mass thereof having a time-dependent water resistance curve which, starting from a high initial strength value of the rapid hardening, shows a negative slope in the first twentyeight days. Granulated blast-furnace slag is admixed to the calcium sulphate alpha -hemihydrate. The quantity of granulated blast-furnace slag is matched to the starting quantity of calcium sulphate alpha -hemihydrate in such a way that, after the rapid hardening, formation of crystalline ettringite and formation of calcium hydrosilicate phases occurs and the time-dependent water resistance curve of the hardened mixture shows a constant positive slope in the first twentyeight days.</p> |
申请公布号 |
FI93827(B) |
申请公布日期 |
1995.02.28 |
申请号 |
FI19890003044 |
申请日期 |
1989.06.21 |
申请人 |
PRO MINERAL GESELLSCHAFT ZUR VERWENDUNG VON MINERALSTOFFEN MBH;SICOWA VERFAHRENSTECHNIK FUER BAUSTOFFE GMBH & CO. KG |
发明人 |
KOSLOWSKI, THOMAS;LUDWIG, UDO;FROEHLICH, ALEXANDER |
分类号 |
C04B28/16;C04B7/32;C04B11/28;C04B28/06;C04B28/14;(IPC1-7):C04B40/00 |
主分类号 |
C04B28/16 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|