Method for recharging a spend fluid catalytic cracking process catalyst |
摘要 |
A zeolitic material with a crystalline structure of MFI type has a ratio of silica to alumina which is lower than 26, and is hydrothermally prepared without organic template reagents or seeding procedures. Crystalline structure is obtained by forming a mixture of a silicon dioxide source, an alkali metal hydroxide, an aluminum source and water, all reactants with the following molar ratios: <IMAGE> <IMAGE> <IMAGE> <IMAGE> where M is an alkali metal, and reacting the mixture at a temperature from 160 DEG to 180 DEG C. for 40-80 hours. The material is characterized by X-ray diffraction, and has good cracking activity and improved selectivity for gasoline octanes.
|
申请公布号 |
US5360774(A) |
申请公布日期 |
1994.11.01 |
申请号 |
US19930103978 |
申请日期 |
1993.08.09 |
申请人 |
INTEVEP, S.A. |
发明人 |
MARTINEZ, NELSON P.;LUJANO, JUAN A.;ALVAREZ, NIEVES;MACHADO, FRANCISCO;LOPEZ, CARMEN M. |
分类号 |
B01J23/92;B01J29/70;C01B39/36;(IPC1-7):B01J29/06 |
主分类号 |
B01J23/92 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|