发明名称 METHOD OF MANUFACTURING AUSTENITE STAINLESS STEEL
摘要 The austenitic manganese steel having a good moldability, strength and weldability is produced by (a) hot and cool rolling a steel slab composed of at most 1.5 wt.% C, 15-35 wt.% Mn, 0.1-6.0 wt.% Al, at least one of at most 0.6 wt.% Si, at most 5.0 wt.% Cu, at most 1.0 wt.% Nb, at most 0.5 wt.% V, at most 0.5 wt.% Ti, at most 9.0 wt.% Cr, at most 4.0 wt.% Ni and at most 0.2 wt.% N, residual Fe and impurity, and (b) annealing it at 550-1000 deg.C for 5 sec. - 20 hr. The austenitic manganese steel is used for cars and electromagnetic panels.
申请公布号 KR940007374(B1) 申请公布日期 1994.08.16
申请号 KR19920013309 申请日期 1992.07.24
申请人 POHANG IRON & STEEL CO., LTD.;KOREA INDUSTRIAL TECHNOLOGY INSTITUTE 发明人 KIM, TAE - UNG;KIM, YONG - KIL;HAN, JAE - KWANG;JANG, RAE - UNG
分类号 C22C38/04;C22C38/06;(IPC1-7):C22C38/04 主分类号 C22C38/04