摘要 |
In accordance with this invention, a gold colored tarnish and corrosive resistant alloy is provided which includes the following: 6 to 20 percent by weight gold, 5 to 10 percent by weight of indium, 5 to 12 percent by weight of palladium, 23 to 40 percent copper, 5 to 10 percent by weight zinc, and 23 to 40 percent by weight silver. It has been found that the aforesaid alloys are sufficiently malleable to be rolled or stamped without fracturing.
|