发明名称 |
COMPOSITION AND PROCESS FOR TREATING TINPLATE |
摘要 |
To impart an excellent corrosion resistance and adherence to the surface of tinplate while avoiding the production of sludge in the treatment bath during continuous treatment, a bath is used thatcontains phosphate ions, from 0.1 to 5.0 g/L of chelating agent, and tin ions; has a pH from 2.0 to 4.5; is essentially free of oxidizing agent and ferric ion; and has an oxidation-reduction potential of </=450 mV more oxidizing than a silver-saturated silver chloride reference electrode. |
申请公布号 |
WO9413855(A1) |
申请公布日期 |
1994.06.23 |
申请号 |
WO1993US11435 |
申请日期 |
1993.12.01 |
申请人 |
HENKEL CORPORATION;AOKI, TOMOYUKI;YOSHIDA, MASAYUKI |
发明人 |
AOKI, TOMOYUKI;YOSHIDA, MASAYUKI |
分类号 |
C23C22/07;C23C22/08;C23C22/23;C23C22/47;(IPC1-7):C23C22/08 |
主分类号 |
C23C22/07 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|