The ceramic humidity sensor manufacturing method comprises the steps of: first calcinating dried powder for one hour at 1,000 deg.C to form a spinel structure; adding K2O of 1-40 weight% in the form of K2CO3 into the calcinated powder; and secondarily calcinating the mixture for one hour at 900 deg.C, thereby increasing conductibility.
|