摘要 |
The invention concerns a method for hydrostatic extrusion of a material 14 made of copper or copper alloy, wherein the material during the extrusion is preheated to a temperature of at least 400 degrees Celsius and provided with a coating containing boron nitride and finely divided silicon dioxide. <IMAGE> |