摘要 |
weaving into the satin woven fabric, using the polyester yarn of ultra fineness of 20-50 denier as a warp, and the splittable fine-denier yarn, whose single fiber's fineness is below 0.2 denier, as a weft so that the density of warps and wefts becomes 10,000-19,000 ea./inch when the weft is splitted, the fabric's thickness and the length of the raised yarn become 0.20-0.40mm, 0.4-0.6mm respectively after the fabric is subjected to the raising process; buffing; and finally resin finishing.
|