摘要 |
<p>PCT No. PCT/EP92/01051 Sec. 371 Date Feb. 1, 1994 Sec. 102(e) Date Feb. 1, 1994 PCT Filed May 13, 1992 PCT Pub. No. WO92/21450 PCT Pub. Date Dec. 10, 1992.The present invention relates to a method of producing dull surfaces, in which initially a first paint layer is applied in a first layer thickness and at least one second paint layer is then applied on top of the first paint layer, at least the paint layer applied last being provided with dulling agents and having a dry film layer thickness which is less than the average particle size of the dulling agent. The method is characterized in that the paint layers applied are cured by ionizing radiation.</p> |