摘要 <p>The specification describes a process for producing synthetic rutile from a titaniferous ore or concentrate. The process involves three basic steps which are reduction, removal of iron by leaching or aeration and removal of other impurities by leaching in a solution of a strong mineral acid such as hydrochloric acid or sulphuric acid. The conditions of reduction are controlled to promote the formation of metallic iron, a major rutile phase and a minor impurity-bearing phase. The minor impurity-bearing phase may be a metatinatate, an anosovite or a pseudobrookite. However, formation of a metatinatate is normally preferred. Suitable reductants include carbonaceous materials or hydrogen bearing gases such as natural gas or synthetic gas. The process is capable of removing more than 80% of each of the contained iron, magnesium and manganese remaining as oxides after reduction. Substantial proportions of contained aluminium can also be removed.</p>
申请公布号 JPH06501741(A) 申请公布日期 1994.02.24
申请号 JP19910505259 申请日期 1991.03.01
申请人 发明人
分类号 C22B3/06;C22B3/08;C22B5/10;C22B5/12;C22B5/14;C22B9/05;C22B34/12;(IPC1-7):C22B34/12 主分类号 C22B3/06
代理机构 代理人
主权项
地址