发明名称 |
Process for producing a composite material consisting of gamma titanium aluminide as matrix with titanium diboride as perserdoid therein. |
摘要 |
<p>A TiA l intermetallic compound source and a boride which is less stable than TiB2 are mixed and melted, followed by solidification to form a TiB2-dispersed TiA l -based composite material in which the TiB2 is contained in an amount of 0.3 to 10% by volume. In this process, the dispersed TiB2 particles become very fine, so that the hardness as well as the elongation and bending strength of the TiA l material are improved by the finely dispersed TiB2 particles.</p> |
申请公布号 |
EP0577116(A1) |
申请公布日期 |
1994.01.05 |
申请号 |
EP19930110479 |
申请日期 |
1993.06.30 |
申请人 |
TOYOTA JIDOSHA KABUSHIKI KAISHA |
发明人 |
MORIKAWA, TAKASHI;SHAMOTO, HIROYUKI;SUGANUMA, TETSUYA |
分类号 |
C22C14/00;C22C1/05;C22C1/00;C22C1/10;C22C29/14;C22C32/00;(IPC1-7):C22C32/00 |
主分类号 |
C22C14/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|