摘要 |
<p>A non-slip composition including a polymer epoxy and aluminum oxide aggregate (18) is applied to a ground surface (10) where lighting conditions may be poor. The epoxy composition including two parts of diglycidyl ether resin and one part aliphatic amine adduct modified with 30 % amyl ethyl piperidine as a stabilizer is applied to the surface in the form of strips (12, 14, 16). A phosphorescent pigment including zinc sulfide and copper may be mixed with the epoxy to provide luminescent characteristics thereto. The aluminum oxide aggregate (18) is spread across the strips (12, 14, 16) prior to curing of the epoxy to enhance the light emitting properties of the phosphorescent pigment and provide a non-slip surface.</p> |