摘要 |
<p>The method for the manufacture of laminated glass containing a metal piece (3) comprises: rinsing of the metal part by means of ultrasounds, the subsequent elimination of the static electricity and putting the glass (2) into a furnace together with a polivinil butiral layer on the glass part and the metal part, a second glass plate (1) being placed on top and submiting the whole assembly to warming up under controlled pressure, submitting the assembly to pressure and temperature up to 8,0 Kg/cm<2> and 135 DEG C, cooling down the assembly to room temperature as a final stage. <IMAGE></p> |