发明名称 ALUMINA-MAGNESIA-ENRICHED SPINEL CARBON BRICKS
摘要 PURPOSE:To provide refractory bricks ensuring an adequate level of permanent linear expansion coefficient comprising an alumina-magnesia-enriched spinel carbon bricks to which electrofused magnesia-enriched spinel starting material reduction in antislugging properties. CONSTITUTION:10 to 80wt.% of an electrofused magnesia-enriched spinel starting material containing more than 95wt.% of the total MgO and Al2O3 at a MgO/Al2 O3 weight ratio of 50/50 to 95/5, 3 to 60wt.% of a carbonaceous starting material and 10 to 85wt.% of an alumina starting material are used for the production.
申请公布号 JPH05238811(A) 申请公布日期 1993.09.17
申请号 JP19920039881 申请日期 1992.02.26
申请人 KAWASAKI REFRACT CO LTD;KAWASAKI STEEL CORP;MITSUBISHI MATERIALS CORP 发明人 NAKAJIMA MASAYOSHI;OKAMOTO TAKAO;SHINTANI HIROTAKA;IMAIDA YASUO;OISHI IZUMI;NANBU MIKI;HANAOKA HARUO
分类号 C04B35/103;C04B35/10;C04B35/44;C04B35/443;C04B35/52 主分类号 C04B35/103